A multilayer PSA construction includes a facestock, a hazy, first adhesive layer adjacent the facestock, and a PSA layer adjacent the first adhesive layer, and is protected until use by a release liner. The first adhesive layer includes an immiscible blend of a first elastomer having a first glass transition temperature and forming a continuous phase, and a second elastomer forming a discontinuous phase. The second elastomer has a glass transition temperature greater than the first glass transition temperature. The first adhesive layer also contains a tackifying component, which is preferentially soluble in the discontinuous phase. The PSA layer has a composition different from the first adhesive layer and is formed of at least one tackified elastomer that provides a measurable third maximum glass transition temperature, which is less than the second glass transition temperature. The multilayer PSA construction exhibits reduced migration of tackifiers and plasticizers over time.
CROSS-REFERENCE TO RELATED APPLICATION
This patent application is a divisional of U.S. patent application Ser. No. 09/158,990 now U.S. Pat. No. 6,183,862, filed Sep. 23, 1998, the entire contents of which is fully incorporated by reference herein.
The present invention is directed to pressure-sensitive adhesive compositions and pressure-sensitive adhesive constructions fabricated using the pressure-sensitive adhesive compositions. The pressure-sensitive adhesive compositions comprise about 10 to about 40% of a styrene-isoprene block copolymer, about 5 to about 30% of a styrene-butadiene block copolymer, about 30 to about 65% of an aromatically modified tackifying resin, about 8 to about 30% of a plasticizing oil and optionally about 0.2 to about 2% of an antioxidant, wherein the percentages are based on the total weight of the composition.
The invention is directed to an ultra thin pressure sensitive adhesive construction suitable for the high speed application of label mounting equipment. The labels include a polyethylene film having a density of from 0.917 to 0.924 g/cm.sup.3 and a thickness of less than 1.8 mils; a pressure sensitive adhesive on one surface of the film; and a release composition coated paper liner having a thickness of less than 2.2 mils releasaby attached to the pressure sensitive adhesive.