or
Bookmark and Share
Method of producing a dielectric ceramic composition
 
   
Document Number
US Patent 7585802
Issued Date
September 8, 2009
Link
Map
Abstract
A dielectric ceramic composition comprised of at least dielectric particles having barium titanate as its main ingredient, wherein the ratio of dielectric particles having a surface diffusion structure comprised of a main ingredient phase comprised of the main ingredient and a diffusion phase present around the main ingredient phase with respect to said dielectric particles is 60% or more and the ratio of dielectric particles having a domain in the main ingredient phase with respect to the dielectric particles having the surface diffusion structure is 20% or less. According to the present invention, a dielectric ceramic composition and electronic device realizing good high temperature accelerated life can be provided.
Tags:
Description:
Amusing 0%
Clever 0%
Complex 0%
Efficient 0%
Historic 0%
Important 0%
Innovative 0%
Interesting 0%
Practical 0%
Simple 0%
Number of Claims:
4
Comments:
no comments yet
Owner
TDK Corporation (Tokyo,JP)
Published
September 8, 2009
Application Number
12/292,042
Filed
November 10, 2008
US Classification
501/139   264/615
Int'l Classification
C04B   35/468   (20060101)  
Examiner
Attorney/Law Firm
Parent Case
This is a Continuation of application Ser. No. 11/604,741 filed Nov. 28, 2006, now abandoned, which in turn claims priority of Japanese Patent Application No. 2005-346881 filed Nov. 30, 2005. The disclosure of the prior application is hereby incorporated by reference herein in its entirety.
Priority Data
Nov 30, 2005 [JP] 2005-346881
USPTO Field of Search
501/139   264/615  
Related Patents
Claims
Description
About| FAQs| Terms & Disclaimer| Link to Us| Contact Us